View Larger Image Continuous cooling precipitation diagram of high alloyed Al-Zn-Mg-Cu 7049A alloy The precipitation behaviour during cooling from solution annealing of high alloyed 7049A aluminium alloy was investigated, covering the complete cooling-rate-range of technical interest. This ranges from slow cooling rates close to equilibrium up to rates above complete supersaturation and is covering seven orders of magnitude in cooling rate (0.0005 to 5000 K/s). Share this:FacebookXLike this:Like Loading... By PhysAdmin|2020-05-17T13:44:37+02:0021st April 2020|Science|0 Comments Share This Story, Choose Your Platform! FacebookTwitterRedditLinkedInWhatsAppTumblrPinterestVkXingEmail About the Author: PhysAdmin Related Posts Precipitation enthalpy during cooling of aluminum alloys obtained from calorimetric reheating experiments Gallery Precipitation enthalpy during cooling of aluminum alloys obtained from calorimetric reheating experiments Interdisciplinary Faculty, LLM Gallery Interdisciplinary Faculty, LLM ResearchGate Profile Gallery ResearchGate Profile Hardware Instructables Gallery Hardware Instructables Leave A Comment Cancel replyComment Save my name, email, and website in this browser for the next time I comment. Δ
Leave A Comment